Cristobalite Investment Materials for Rapid Heating
Accurate casting investment material for gold and palladium alloys.
Packing | 3 kg |
---|
Powder/Water Mixing Ratio, g:mL | 100 : 35 |
---|---|
Hardening Time | 15 min |
Hardening Expansion, % | 0.5 |
Thermal Expansion, % | 1.4 |
Compression Strength, MPa | 4.0 |