Category
Synthetic Resin

ORTHO BRIGHT COLOR

ORTHO BRIGHT COLOR

Self-Curing Resin for Orthodontic Applications

Features
  • Hardening time for complete polymerization reaction extends to about 8 minutes allowing for sufficient working time.
  • Liquid monomer diffuses into the interstices of the polymer beads – releasing tension – migrates evenly and then absorbs by the matrix to form a homogenous fluid state.
    Diffusion of the liquid is like percolation of water into the sand.
    Excellent viscosity prevents the mixture fluid from sagging or slopping allowing for accurate control and shaping.
  • Superior hardness ideal for orthodontic applications.

 

Usage All types of Splint
Functional Orthodontic Appliances
Deciduous Dentures
Temporary Dentures
Individual Trays
Packing 1-1Set
(Starter Kit)
Retail
Powder 50 g (x 5 color) 250 g
Liquid 70 mL 250 mL
Accessories (Silicon Cup, Cylinder Cup, Pipette, Shade Guide) X 1 Each; Pipette Nozzle X 3 Pipette x 1
Color ORTHO BRIGHTORTHO BRIGHT COLORORTHO BRIGHT COLORORTHO BRIGHT COLORORTHO BRIGHT COLOR

 

Physical Properties
Post Setting Shrinkage,
(23℃)
Mud or sand-like state 1min 30sec
Dough state 7min 30sec
Rubbery, Cured state 8min
Flow of Mixture in Wet Condition(cm) 10.3
Vickers Hardness, Hv 13.3

 

Methods of Use

Sprinkle Technique. Apply a separating agent for denture base to a plaster model.
Perform preparation such as wax relief and fixing wires.
Sprinkle liquid onto the powder until basement is formed.
When the shine of the resin has disappeared, form the model using fingers.
When resin elasticity is felt, immerse in water at 40-50℃ (Placing in a pressure pot is recommended in order to minimize air bubble formation.)

Mixing Technique.
Measure appropriate amount of powder and liquid.
Put powder into liquid and mix using spatula or mixing stick.
Mix slowly to avoid air bubble formation. When the mix has turned into paste-like body, pour into model.
When the shine of the resin has disappeared, form the model using fingers.
Use Sprinkle Technique for narrow parts.
When resin elasticity is felt, immerse in water at 40-50℃ (Placing in a pressure pot is recommended in order to minimize air bubble formation.)

Resin Packing Technique.
Follow Mixing Technique for preparation.
When the resin reaches the doughy state, immediately pack into the flask.
Press the flask by hydraulic press until polymerization is complete (operate pressing before the curing process starts, refer to hardening time).

Brush On Technique.
Put appropriate amount of powder and liquid to their corresponding containers.
Wet the tip of the brush and dip into the powder.
Take desired amount of powder to suffice powder load.
Stack the load mixture until desired amount is achieved.
Let hard-polymerize.
Bigger brush is recommended for efficient results.